تفاعل #54212

ord-0708d5af58984a5f8a2d2c83dc6c2c80

معادلة التفاعل

CC(C[*:1])[*:2]
polypropylene
C=C(C)C(=O)O
methacrylic acid
C=CC
propylene
C=C(C)C(=O)O
methacrylic acid

الكواشف

لا شيء

المذيبات

ظروف التفاعل

درجة الحرارة
95°CELSIUS
الظروف التفصيلية
See reaction.notes.procedure_details.

المعالجة

  1. 1
    درجة الحرارةThe mixture was then heated at just
  2. 2
    ترشيحThe product was filtered
  3. 3
    غسيلwashed with water
  4. 4
    أخرىdried in a vacuum oven at 75° C. for two hours

الإجراء التجريبي

A modified resinous polymer of propylene containing approximately 10% by weight methacrylic acid was prepared as follows: 0.5 grams of Lupersol 256 Peroxide (peroxyhexanoic acid manufactured by Wallace & Tiernan Inc., Lucidol Division) was added to a reactor containing 200 grams of substantially crystalline homopolymeric polypropylene powder, 25 grams of methacrylic acid and 600 grams of water. The mixture was then heated at just below reflux temperature, about 95° C., for one hour. The product was filtered and washed with water followed by acetone and then dried in a vacuum oven at 75° C. for two hours. The modified resinous polymer of propylene weighed 225.6 grams.

المصدر

DOI: 10.6084/m9.figshare.5104873.v1براءة الاختراع: US04147741uspto-grants-1979_04