تفاعل #44308

ord-0d1d811887594b48876707271c6f6132

المتفاعلات

المذيبات

ظروف التفاعل

الظروف التفصيلية
See reaction.notes.procedure_details.

المعالجة

  1. 1
    أخرىA reactor equipped with an exhaust vent
  2. 2
    أخرىfollowed by polymerization at 190° C. for 24 hours
  3. 3
    أخرىAfter the reaction
  4. 4
    أخرىpurified by precipitation in methanol

الإجراء التجريبي

A reactor equipped with an exhaust vent and a thermometer was charged with 263 g of L-lactide (reagent, supplied by SIGMA-ALDRICH JAPAN K.K.), 42 g of glycollide (prepared under the same conditions as those in Example 1), 194 g of ε-caprolactone (reagent, supplied by TOKYO CHEMICAL INDUSTRY CO., LTD.) and 0.01 g of tin octanoate (reagent, supplied by SIGMA-ALDRICH JAPAN K.K.) as a catalyst, and the pressure inside the reactor was reduced to 1×10−3 mmHg with a vacuum pump, followed by polymerization at 190° C. for 24 hours. After the reaction, a copolymer was dissolved in chloroform and purified by precipitation in methanol, to give a lactic acid/glycolic acid/ε-caprolactone copolymer.

المصدر

DOI: 10.6084/m9.figshare.5104873.v1براءة الاختراع: US07736393B2uspto-grants-2010_06