المعالجة

  1. 1
    أخرىwas prepared
  2. 2
    درجة الحرارةheated for thermal polymerization

الإجراء التجريبي

A 10 μm-thick nonwoven fabric made of polyethylene (PE) was prepared. Then, divinylbenzene and lithium (Li) styrenesulfonate were impregnated in the fabric and then heated for thermal polymerization, resulting in formation of a thin-film of 10 μm thick with a copolymer of sulfonyl group-owning styrene and divinylbenzene being impregnated in the nonwoven fabric. This was cut into a portion having the cell size, which was then put on the EC layer.

المصدر

DOI: 10.6084/m9.figshare.5104873.v1براءة الاختراع: US07184191B2uspto-grants-2007_02