تفاعل #335952
ord-b83584e673d14dd995e2cecdf1a93ef9
الكواشف
لا شيء
ظروف التفاعل
الظروف التفصيلية
See reaction.notes.procedure_details.
المعالجة
- 1workup.ADDITIONdehydration of the thickener in an open kettle sufficient mineral oil was added
- 2أخرىwas 407° F.
- 3أخرى(208° C.)
الإجراء التجريبي
A lithium hydroxystearate grease thickener was prepared by saponification of a mixture containing 12-hydroxystearic acid (50%) and the tri-glyceride thereof (25%) and 25% of C22 fatty acids containing no OH groups with lithium hydroxide in a mineral oil vehicle (ISO 150 viscosity grade of a 70/30 mixture of naphthenic and paraffinic stocks) at about 350° F. in a closed contactor. After depressuring and dehydration of the thickener in an open kettle sufficient mineral oil was added to reduce the thickener content to about 8%. The dropping point of this grease was 407° F. (208° C.). This grease contained no phosphorus or sulfur additives.