تفاعل #2146739

ord-7015cf9b3913433e80581de2abcb85d2

معادلة التفاعل

C=C(C)C(=O)OCCN(C)C
dimethylaminoethyl methacrylate
C=CC(=O)O
acrylic acid
C=C(C)C(=O)OCCN(C)C.C=CC(=O)O
dimethylaminoethyl methacrylate acrylic acid

الكواشف

لا شيء

المذيبات

ظروف التفاعل

درجة الحرارة
71°CELSIUS
الظروف التفصيلية
See reaction.notes.procedure_details.

المعالجة

  1. 1
    أخرىA relative permeability modifier useful in the present invention was prepared
  2. 2
    أخرىsparging with nitrogen for 30 minutes
  3. 3
    workup.ADDITIONfollowed by the addition of 0.2 mL of 2-mercaptoethanol and 1.3 g of 2,2′-azo bis(2-amidinopropane)dihydrochloride

الإجراء التجريبي

A relative permeability modifier useful in the present invention was prepared as follows. First, a polymer was made by mixing 45.0 g of dimethylaminoethyl methacrylate, 6.8 g acrylic acid, 372.0 g of water and sparging with nitrogen for 30 minutes. Thereafter, the pH was adjusted to approximately 5.3 with 5.7 mL of concentrated sulfuric acid, followed by the addition of 0.2 mL of 2-mercaptoethanol and 1.3 g of 2,2′-azo bis(2-amidinopropane)dihydrochloride. The resulting solution was then heated to 71° C., with stirring, and held for 18 hours to produce poly(dimethylaminoethyl methacrylate/acrylic acid).

المصدر

DOI: 10.6084/m9.figshare.5104873.v1براءة الاختراع: US08278250B2uspto-grants-2012_10