تفاعل #1580053
ord-952d1af47cfe43f287a70b72498e01ab
معادلة التفاعل
الكواشف
ظروف التفاعل
درجة الحرارة
188°CELSIUS
الظروف التفصيلية
See reaction.notes.procedure_details.
المعالجة
- 1أخرى, hereafter abbreviated T-9) (1.35×10-2 g, 3.3×10-5 moles) were combined in a stirred reactor at 182° C
- 2workup.ADDITIONwas added
- 3درجة الحرارةthe temperature was increased to 200° C
- 4workup.WAITAfter 45 minutes
الإجراء التجريبي
Polymerization grade 1,3-dioxan-2-one (trimethylene carbonate, hereafter abbreviated TMC) (97.5 g, 0.995 mole), diethylene glycol (hereafter abbreviated DEG) (4.20×10-2 g, 4.0×10-4 mole), and Dabco T-9 catalyst (a stannous 2-ethylhexanoate catalyst formulation sold by Air Products, Inc., hereafter abbreviated T-9) (1.35×10-2 g, 3.3×10-5 moles) were combined in a stirred reactor at 182° C. The temperature was raised to 188° C. and the mixture was stirred for 11/2 hours at this temperature. Polymerization grade l-lactide (52.5 g, 0.364 mole) was added and the temperature was increased to 200° C. After 45 minutes, the polymer was discharged from the reactor and allowed to solidify.